Welcome to the BURGMANN Sealing World
Resin-impregnated carbons

display greater chemical resistance than metal-impregnated carbons, but their strength values are inferior. The temperature operating limit lies at approximately 220 °C, and at around 150 °C when used as face material.

 

Blistering on a resin-impregnated carbon seal face

f133-1.jpg (11071 bytes)